If the horse mouth iron box printing appears anti-sticky problem how to solve?

* 来源: Good Torch Enterprise Corp. * 作者: twa133 * 发表时间: 2018/12/27 13:24:11 * 浏览: 275
If the horse mouth iron box printing appears anti-sticky problem how to solve?The first thing to 
know is why this problem occurs:

1, the drying is not sufficient, the residual solvent is many.In particular, the printing plate is deeper 
and the use of slow-drying solvents in the case.
2, Horse mouth iron box printing after drying film cooling is not sufficient, or the pressure when 
the winding is too large.
3, gloss, silver ink printing, easy to appear inadequate drying phenomenon, resulting in sticky ink.

Solution to the problem of anti-viscosity in the printing of horse mouth iron box
1. Keep the drying system in optimal condition, dry temperature, air volume, wind speed is 
appropriate, and match the printing speed, fully reduce residual solvents.
2, check whether the cooling system is in good working condition, so that the film rewinding when
 fully cooled.The winding tension and winding pressure should be appropriate and, if necessary, 
reduce the number of rice collected.
3, gloss, silver ink printing to reduce the printing speed, full drying